Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 510 MPa @Temperature 21.1 °C |
74000 psi @Temperature 70.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K 8HS Carbon Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Strength | 510 MPa | 74000 psi | |
Performance Alloys MoldStar® 22 (PAS 22) Bronze Mold Alloy Description: MoldStar® 21 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: Ejector SleevesLifter BladesThin Wall Appli.. |