Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 500 MPa | 72500 psi | ASTM C-773-88 / DIN 51067T1 |
CeramTec Sikor® E Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Compressive Strength | 500 MPa | 72500 psi | ASTM C-773-88 / DIN 51067T1 |
CeramTec Sikor® S Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Compressive Strength | 500 MPa @Thickness >=5.00 mm |
72500 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |
|||
Compressive Strength | >= 500 MPa | >= 72500 psi | Ambient |
China-Yixing Longly Refractories 95 Alumina Ceramic Seals LONGLY's alumina ceramic seals (alumina accounts for 95-99%) can be finished by mirror-polishing process. Because of high mechanical strength, strong chemical corrosion resistance, good air tightne.. |
|||
Compressive Strength | >= 500 MPa | >= 72500 psi | Ambient |
China-Yixing Longly Refractories 95 Alumina Ceramic Tubes & Rods LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat.. |
|||
Compressive Strength | 500 MPa | 72500 psi | |
Pyrotek Pyromat TS-045 Electrical Insulating Board Pyromat TS-045 is a black laminate, press molded from high-temperature thermoset resin and reinforced with glass filament mat. Its composition ensures excellent chemically resistance and antistatic.. |
|||
Compressive Strength | >= 500 MPa | >= 72500 psi | Ambient |
China-Yixing Longly Refractories 95 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |