Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 71.7 MPa | 10400 psi | ASTM D695 |
ITW Devcon Plastic Steel® Metal Repair 5 Minute® Putty (SF), Dark Grey Information provided by ITW Devcon |
|||
Compressive Strength | 71.7 MPa | 10400 psi | ultimate load |
BNZ Materials Transite HT Low Temperature Industrial Board These non-asbestos, monolithic fiber cement industrial boards are used in environments up to 1000°F where high strength is the primary concern. These fiber cement boards are used in the foundry ind.. |