Polymer Property : Compressive Strength = 71.1 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength <= 0.490 MPa
<= 71.1 psi
Cold Crushing Strength
Chosun Refractories A-2 Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength <= 0.490 MPa
<= 71.1 psi
Cold Crushing Strength
Chosun Refractories A-3 Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength <= 0.490 MPa
<= 71.1 psi
Cold Crushing Strength
Chosun Refractories A-1 Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).