Mechanical Properties Metric English Comments
Compressive Strength 48.3 - 51.7 MPa
7010 - 7500 psi
ASTM C133
Ceradyne Thermo-Sil® HS Fused Silica
Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi..
Compressive Strength 48.3 - 51.7 MPa
7010 - 7500 psi
ASTM C133
Ceradyne Thermo-Sil® Castable 220 Fused Silica
Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi..