Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 7.50 MPa | 1090 psi | EN 1094-5: 1995 |
Skamol Group Moler LR-1750 Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |