Mechanical Properties Metric English Comments
Compressive Strength 48.0 - 51.0 MPa
6960 - 7400 psi
Pyrotek Dense Fused Silica Pre-Cast Shapes
Pyrocast Dense Fused Silica is an economical product for shapes demanding thermal shock resistance at temperatures. Pyrocast DFS stands up to repeated use in molten metal casting in aluminum, coppe..
Compressive Strength 48.0 MPa
6960 psi
with grain
Pyrotek PT-10 Graphite
PT-10 Graphite offers the highest resistance to oxidation available. Its unique composition gives it the most durable, long lasting, oxidation resistant properties available from treated graphite.A..
Compressive Strength 48.0 MPa
6960 psi
cured at 540°C
Pyrotek Pyrocast AR-S Castable Refractory
Pyrocast AR-S is a low cement, fused silica, castable refractory which exhibits excellent resistance to thermal shock. It is inert to liquid aluminum and its alloys. It is a high strength material..
Compressive Strength 48.0 MPa
6960 psi
5% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Conditioned
Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 48.0 MPa
6960 psi
5% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Dry
Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 48.0 MPa

@Time 3.60e+7 sec
6960 psi

@Time 10000 hour
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre..
Compressive Strength 47.99 MPa
6960 psi
CMT Materials HYTAC® C1R Highly Durable Syntactic Foam, Dust-Free Machining/Polishing
HYTAC-C1R is easily machined without the dust typically associated with epoxy syntactic foam. This new copolymer base has been optimized for both the machine shop and the thermoforming process.Exce..