Polymer Property : Compressive Strength = 682000 psi
Polymer Property :
Compressive Strength =
682000 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Compressive Strength
4700
MPa
682000
psi
DIN 51067T1
CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2
DC 25 is a ZTA Alumina Zirconia Platelet Composite used in dental applications.