Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 68.6 MPa | 9960 psi | Cold Crushing |
Sharadaa Ceramics PCF40 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Compressive Strength | 68.6 MPa | 9960 psi | Cold Crushing Strength |
Chosun Refractories AH-4 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 68.6 MPa | 9960 psi | Cold Crushing Strength |
Chosun Refractories AH-5 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 68.6 MPa | <= 9960 psi | Cold Crushing Strength |
Chosun Refractories CUN-669 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 68.6 MPa | <= 9960 psi | Cold Crushing Strength |
Chosun Refractories HAL-SNA Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 68.6 MPa | 9960 psi | Cold Crushing Strength |
Chosun Refractories HSC-16HW Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 68.6 MPa | 9960 psi | Cold Crushing Strength |
Chosun Refractories KSB-A65 Special Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 68.6 MPa | 9960 psi | Cold Crushing Strength |
Chosun Refractories SAL70 Special Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 68.6 MPa | 9960 psi | Cold Crushing Strength |
Chosun Refractories SAL75 Special Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 68.6 MPa | 9960 psi | Cold Crushing Strength |
Chosun Refractories SC40 Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 68.6 MPa | 9960 psi | Cold Crushing Strength |
Chosun Refractories SF35 Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 68.6 MPa | 9950 psi | Peak Stress, cured for 16 hrs at 21-27°C + post cured for 1 hrs at 82°C, 13 mm/min; ASTM D695-10 |
3M Scotch-Weld™ EC-2815 B/A FR Epoxy Adhesive 3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a two-component epoxy adhesive with cure at room temperature or with additional heat to form a tough, impact-resistant bond. It has excellent adhesion.. |