Polymer Property : Compressive Strength = 66.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 66.2 MPa
9600 psi
ASTM D695
BCC Products Kwik Kast BC 8645 Urethane Casting
BCC Kwik Kast/Gray is a two component, fast setting polyurethane reproduction plastic. BC8645 has been reformulated to enhance filler suspension and avoid hard packing @ 77ºF. Uses include; tracing..