Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | >= 4.50 MPa | >= 653 psi | perpendicular to plane; ISO 844 |
3A Composites Core Materials AIREX® C70.200 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli.. |
|||
Compressive Strength | 4.50 MPa | 653 psi | EN 1094-5: 1995 |
Skamol Group SKAMOLEX V-1100 (700) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Compressive Strength | 4.50 MPa | 653 psi | EN 1094-5: 1995 |
Skamol Group SKAMOLEX V-1100 (700) Panel Design SKAMOLEX panel designs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and versatil.. |