Polymer Property : Compressive Strength = 58.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 58.9 MPa
8540 psi
ASTM D695
ITW Devcon Metal Repair Bronze Putty (BR), Bronze
Information provided by ITW Devcon