Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 56.0 MPa | 8120 psi | 10% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 1200 Cast Polyamide 12, Dry Application: sprockets, chain-wheels, pulleys, wheels, slide and seal rings, curve disks, etc.Information provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 56.0 MPa | 8120 psi | 5% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Conditioned Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 56.0 MPa | 8120 psi | 5% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Dry Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 56.0 MPa | 8120 psi | 5% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 510 Polyethylene Terephthalate Application: friction bearings, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 56.0 MPa | 8120 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |