Mechanical Properties Metric English Comments
Compressive Strength 48.3 - 55.2 MPa
7000 - 8000 psi
Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, ..