Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.380 MPa | 55.1 psi | average; perpendicular to plane; ISO 844 |
3A Composites Core Materials AIREX® R63.50 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with high damage tolerance. This one of a kind formula combines very high elongation and excellent bond strength. AIREX® R63 is cold.. |