Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 50.3 MPa | 7300 psi | |
Abatron ROCKWELD 55-27 A/B Structural Adhesive Putty; Epoxy ROCKWELD 55-27 is a 2-component epoxy system with low density, high-strength, and no shrinkage. It is a structural adhesive putty for sculpturing, repairs and restoration of stone, concrete and maso.. |