Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 5.30 MPa | 769 psi | EN 1094-5: 1995 |
Skamol Group SKAMOLEX V-1100 (800) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Compressive Strength | >= 5.30 MPa | >= 769 psi | perpendicular to plane; ISO 844 |
3A Composites Core Materials AIREX® C70.250 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |