Mechanical Properties Metric English Comments
Compressive Strength 34.0 MPa
4930 psi
Aremco Ceramacast™ 673 Castable Ceramic
Chemical setting. Two-part ceramic exhibiting high thermal conductivity. Used to pot small temperature sensors, gas igniters, and high intensity lights. Applied in areas up to 1" diameter by 1" de..
Compressive Strength 34.0 - 69.0 MPa
4930 - 10000 psi
ASTM D695
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Compressive Strength 34.0 - 69.0 MPa
4930 - 10000 psi
ASTM D695
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, ..