Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 333 MPa | 48400 psi | Cold Crushing Strength |
Chosun Refractories APB-4 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |