Mechanical Properties Metric English Comments
Compressive Strength 3320 MPa
482000 psi
PSM Industries Ferro-TiC® CM High Chrome Tool Steel
Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.For ..