Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 3120 MPa | 453000 psi | |
PSM Industries Ferro-TiC® CS-40 Martensitic Stainless Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.High.. |