Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.303 MPa | 44.0 psi | 10% Deformation; Green |
Unifrax Fiberfrax® Duraboard® 3000 Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |
|||
Compressive Strength | 0.303 MPa | 44.0 psi | 50% deformation |
Unifrax Fiberfrax® 880 Ceramic Fiber Paper 880 paper is made from a higher alumina content, shorter, smaller diameter fiber and laid up at higher densities. These product parameters lead to reduced shrinkage, higher strength, an increased o.. |