Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 43.2 MPa | 6270 psi | cured at 650°C |
Pyrotek Pyrocast AR FINE Castable Refractory Pyrocast AR Fine is a fine-grain fused silica castable, offering similar insulation properties, yet lighter weight that the Pyrocast AR formulation. Pyrocast AR Fine is suited for thin wall casting.. |