Mechanical Properties Metric English Comments
Compressive Strength 410 MPa
59500 psi
ISO 604
Sumitomo Bakelite North America RX® 655 Novolac Phenolic
Fiberglass and mineral reinforced phenolic molding compound with very high fill level (75%). Excellent dimensional stability and good strength at elevated temperatures. Very low thermal expansion ..