Polymer Property : Compressive Strength = 404 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 404 MPa
58600 psi
10 oz glass cloth laminate
BCC Products BC 5105 Epoxy Laminating System
BC 5105 is a clear, unfilled, low viscosity laminating system. This heat resistant resin exhibits excellent wet out, reasonable working time and may be used at room temperature without post-curing. ..