Polymer Property : Compressive Strength = 400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 2.76 MPa
400 psi
BNZ Materials 2861LI Insulating Aggregate
BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i..
Compressive Strength 2.76 MPa
400 psi
3M S22 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Compressive Strength 2.76 MPa
400 psi
BNZ Materials 2653LI Insulating Aggregate
BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i..