Mechanical Properties Metric English Comments
Compressive Strength 40.5 MPa

@Strain 3.50 %
5870 psi

@Strain 3.50 %
DIN EN ISO 604
Wolf Kunststoff ZEDEX® ZX-530KF15 A5M Polymer Alloy
Main Characteristics: High elongation; High impact strength; Stress resistantApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInformation provided by Zed..