Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 4.10 MPa | 595 psi | Thickness |
Pyrotek PTB 2200 Structural Board ApplicationsCaster tips Small machined nozzles Slotted caster tips AdvantagesHigh strength Resistant to thermal shock Easily machined Non-wetting to molten non-ferrous metals Low thermal mass High t.. |