Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 27.2 MPa | 3950 psi | |
Engineered Syntactic Systems BZ-26 Deep Water Syntactic Foam Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having.. |