Mechanical Properties Metric English Comments
Compressive Strength 26.9 MPa
3900 psi
10% Def.; ASTM D695
Quadrant EPP Armor-X™ Non-Marring, Elastomer Polymeric Blend (ASTM Product Data Sheet)
Compressive Strength 26.9 MPa
3900 psi
ASTM D695
PolyOne Lubri-Tech™ NL-30GF/15T Nylon 6/12, Glass Filled, PTFE Lubricated  (discontinued **)