Polymer Property : Compressive Strength = 39.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 29.4 - 39.2 MPa
4270 - 5690 psi
Cold Crushing
Sharadaa Ceramics HA 60 High Alumina Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 29.4 - 39.2 MPa
4270 - 5690 psi
Cold Crushing
Sharadaa Ceramics HH 40SD Normal Medium and High Heat and Super Duty Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 29.4 - 39.2 MPa
4270 - 5690 psi
Cold Crushing
Sharadaa Ceramics HH 45 Normal Medium and High Heat and Super Duty Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 29.4 - 39.2 MPa
4270 - 5690 psi
Cold Crushing
Sharadaa Ceramics HA 50 High Alumina Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..