Polymer Property : Compressive Strength = 3840 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 26.5 MPa
3840 psi
1% Deformation; ASTM D-695
UBE UPIMOL® R Polyimide Shape
Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub..
Compressive Strength 26.5 MPa

@Temperature 1350 °C,
Time 10800 sec
3840 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories CRS-50 Blast Furnace Tap-Hole Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).