Compressive Strength 3800 MPa
551000 psi
Sapco 99.9% Aluminum Oxide
Information provided by Sapco.
Compressive Strength 3800 MPa
551000 psi
CeramTec Rubalit® A 1898 Alumina, 98%
Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond ..