Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | <= 21.6 MPa | <= 3130 psi | Cold Crushing Strength |
Chosun Refractories IC-S Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |