Mechanical Properties Metric English Comments
Compressive Strength 3000 MPa
435000 psi
Sapco Silicon Nitride, Si3N4
Information provided by Sapco.
Compressive Strength 3000 MPa
435000 psi
DIN 51067T1
CeramTec SL 200 BG Silicon Nitride, Si3N4-Y2O3
SL 200 BG is a silicon nitride ceramic used to make welding rollers, pins, and components, gas nozzles, and forming tools. Silicon nitrides are ideal for components working under mechanical loads an..
Compressive Strength 3000 MPa
435000 psi
ASTM C-773-88 / DIN 51067T1
CeramTec SL 200 ST Silicon Nitride, Si3N4-Y2O3
SL 200 ST is a silicon nitride ceramic especially suitable for components exposed to mechanical stress and engine-specific applications even at elevated temperatures. It is recognized for its high s..
Compressive Strength 3000 MPa
435000 psi
DIN 51067T1
CeramTec SL 303 Silicon Nitride, SiAION+SiC
SL 303 is a silicon nitride ceramic. Silicon nitrides are ideal for components working under mechanical loads and engine parts, even and especially at elevated temperatures. Their property profile i..
Compressive Strength 3000 MPa
435000 psi
Rc0.2; at HRC=64
Bohler-Uddeholm UDDEHOLM Vancron 40 nitrided powder tool steel
Description: Uddeholm Vancron 40 is a nitrided powder tool steel, which means that a “surface coating” is already integrated into the finished tooling material. The result is a tool surface with v..
Compressive Strength 3000 MPa
435000 psi
ASTM C-773-88 / DIN 51067T1
CeramTec 848 Zirconia, ZrO2•MgO
Tetragonal zirconia exhibits high flexural strength and superior low temperature stability. It features higher impact strength and erosive wear resistance as compared to alumina. 848 TTZP (yellow) i..
Compressive Strength 3000 MPa
435000 psi
DIN 51067T1
CeramTec Rubalit® IS 95 Brown Alumina
Rubalit® IS 95 brown is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at..
Compressive Strength 3000 MPa
435000 psi
CeramTec SL200B Silicon Nitride
SL200B ceramic material was designed especially for use in the field of welding technology. SL200B is a 100 bar gas-pressure sintered silicon nitride (Si3N4) with impressive properties. It boasts de..