Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.200 MPa | 29.0 psi | to 10% deformation |
Pyrotek MT-29P Microporous Panel Insulation MT-29P is a unique panel insulation which offers exceptionally low thermal conductivity. The exterior of the panel is a glass fabric which maximizes the strength of the rigid interior panel.Applica.. |
|||
Compressive Strength | 0.200 MPa | 29.0 psi | to 10% deformation |
Pyrotek MT-29Q Quilted Microporous Insulation MT-29Q is quilted to encapsulate its microporous core between glass cloth. The result is a flexible insulating material which offers exceptionally low thermal conductivity. The quilting maintains .. |
|||
Compressive Strength | 0.200 MPa | 29.0 psi | to 10% deformation |
Pyrotek MT-29L Microporous Ladle Lining Insulation MT-29L is a microporous insulation material covered with a flexible glass fabric. Parallel-stitched for ease of handling during installation, it is designed for use between ladle shells and the bac.. |
|||
Compressive Strength | 0.200 - 0.300 MPa @Strain 10.0 % |
29.0 - 43.5 psi @Strain 10.0 % |
DIN EN 826 |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |