Polymer Property : Compressive Strength = 2890 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 2890 MPa
419000 psi
ASTM C-773-88 / DIN 51067T1
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
950 has a combination of high strength (from zirconia) and high hardness (from the alumina phase). It has excellent wear resistance, both in sliding and abrasive conditions. This material offers a g..