Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1900 MPa | 275000 psi | 55 HRC |
Schmolz + Bickenbach Cryodur® 2379 (D-2) Cold Work Die Steel Description: Cryodur® 2379 is a high carbon, high chromium tool steel developed for high wear applications and Supplied in the annealed conditionCharacteristics: Excellent abrasive wear resistance;.. |