Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.180 MPa | 26.1 psi | f<sub>cd</sub>; DIBT Z-23.34-13525 |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Compressive Strength | 0.180 MPa | 26.1 psi | s<sub>perm</sub>; DIBT Z-23.34-13525 |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |