Mechanical Properties Metric English Comments
Compressive Strength 134 - 162 MPa
19500 - 23500 psi
Bulk Molding Compounds BMC T14 General Purpose Molding Compound
BMC T14 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T14 is well suited for injection, transfer or compression molding of intricate parts. Typica..
Compressive Strength 134 - 162 MPa
19500 - 23500 psi
Bulk Molding Compounds BMC A50-MS General Purpose Molding Compound
BMC A50-MS is a medium strength, high appearance, general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A50-MS is well suited for injection, transfer or compres..