Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1600 MPa | 232000 psi | DIN 51067T1 |
CeramTec ZN 40 Zirconia, ZrO2-MgO ZN 40 is a zirconium oxide ceramic with an excellent surface finish and a higher strength than aluminum oxide. Its good crack resistance and anti-friction properties, combined with steel-like therma.. |