Polymer Property : Compressive Strength = 232 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 232 MPa
33600 psi
ISO 604
Vyncolit Neopreg Kinel® SK60 L8G Glass Fiber Reinforced Molding Compound
High flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited fo..