Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 153 MPa | 22200 psi | ASTM D695 |
Plenco 1501 Polyester, Briquette, Compression Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Compressive Strength | 153 MPa | 22200 psi | ASTM D695 |
Plenco 4466 Phenolic, Granular, Compression Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |