Polymer Property : Compressive Strength = 218 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 218 MPa
31600 psi
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP EC008APQ PEI
LNP* THERMOCOMP* EC008APQ is a compound based on Polyetherimide containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, High Flow.
Compressive Strength 218 MPa
31600 psi
ASTM D695
Plenco 7500 Phenolic, Granular, Transfer Molded
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi..