Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 138.01 MPa | 20016 psi | Cold Crushing after 1560°F |
Stellar Canada CERAMITE® CSA Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |