Mechanical Properties Metric English Comments
Compressive Strength 197 MPa
28600 psi
ASTM D695
Plenco 4349 Phenolic, Granular, Transfer Molded
PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer ..
Compressive Strength 197 MPa
28600 psi
ASTM D695
Plenco 4311 Phenolic, Granular, Transfer Molded
PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized..