Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 19.00 MPa | 2755 psi | |
3M Scotchkote™ PR 504 Urethane Pipe Repair Scotchkote Urethane Pipe Repair PR 504 is a special fast curing moisture activated repair bandage for repair bandage for repairs to leaking pipes.Product Features:Easy to apply, requiring no special.. |