Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1620 MPa | 235000 psi | 55 HRC |
Schmolz + Bickenbach Cryodur® 2357(S-7) Cold Work Die Steel Description: Cryodur 2357 is a shock resistant tool steel with excellent toughness and high strength; Suitable for cold and hot work applications up to 1000 °F; and Supplied in the annealed conditi.. |