Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 1500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 10.3 MPa
1500 psi
Break; TM R050-38
Resinlab® EP1287 Filled, Flame Retardant Epoxy Syntactic Foam
Resinlab™ EP1287 is a two part filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-extinguishin..
Compressive Strength 10.3 - 20.7 MPa
1500 - 3000 psi
Crush Strength
Trelleborg Fillite® 160 Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 10.3 - 20.7 MPa
1500 - 3000 psi
Crush Strength
Trelleborg Fillite® 52/7S (355) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 10.3 - 20.7 MPa
1500 - 3000 psi
Crush Strength
Trelleborg Fillite® FG (300) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 10.3 - 20.7 MPa
1500 - 3000 psi
Crush Strength
Trelleborg Fillite® 106 Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 10.3 - 20.7 MPa
1500 - 3000 psi
Crush Strength
Trelleborg Fillite® SG (500) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 10.3 - 20.7 MPa
1500 - 3000 psi
Crush Strength
Trelleborg Fillite® PG (300LF) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Copyright © lookpolymers.com All Rights Reserved