Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 144 MPa | 20900 psi | ASTM D695 |
Plenco 5118 Phenolic, Granular, Transfer Molded PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorptio.. |